Vacuum Reflow Furnace
Vacuum Reflow Furnace
Alternate Name
SST
Manufacturer
Scientific Sealing Technology
Model
3130
Type
commercial
Comments
Fluxless optical fiber and lid sealing.
Void-free die attach.
Temperatures to 500 C