| Tegal 803 | |
|---|---|
| Model | |
| Type | |
| Equipment Characteristics | |
| Wafer diameter(s) List or range of wafer diameters the tool can accept | 100 mm | 
| Wafer holder Device that holds the wafers during processing. | alumina | 
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). | silicon | 
| Wafer thickness List or range of wafer thicknesses the tool can accept | 400 .. 600 µm | 