K&S 798 Automatic 8 inch wafer saw |
|
|---|---|
| Model | Automatic 8 inch wafer saw |
| Type | commercial |
| Equipment Characteristics | |
| Batch sizes | 25 .. 200 mm: 1 |
| MOS clean | no |
| Wafer diameter(s) List or range of wafer diameters the tool can accept |
25 .. 200 mm |
| Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat, no-flat, notched |
| Wafer holder Device that holds the wafers during processing. |
vacuum chuck |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
fused silica, gallium arsenide, glass (category), Pyrex (Corning 7740), quartz (fused silica), quartz (single crystal), silicon, silicon on insulator |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
50 .. 1000 µm |