  Polysilicon RIE
Process characteristics:
must be 0.01 .. 3 µm
0.01 .. 3 µm
Etch rate 0.22 µm/min
Gas Cl2, HBr, SF6, He
Material polysilicon
Primary material removal rate divided by removal rates of secondary materials (i.e., factors by which primary material is removed faster than secondary materials)
photoresist (category): 3, polysilicon: 1
Sides processed either
Temperature 60 °C
Uniformity 0.05
Wafer size
Wafer size
Equipment LAM 9400
Equipment characteristics:
Batch sizes 150 mm: 1
Wafer geometry
Types of wafers this equipment can accept
Wafer holder
Device that holds the wafers during processing.
electrostatic chuck
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
fused silica, Corning Eagle 2000, silicon, Corning 1737, silicon on insulator
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 900 µm