SU-8 pre-bake: View
Process Hierarchy
Bonding
Clean
Consulting
Deposition
Doping
Etch
LIGA
Lift off
Lithography
Mask making
Metrology
Miscellaneous
Packaging
Polishing
Process technologies
Thermal
Anneal
Bake
Oxidation
Unique capabilities
If you are interested in this process, either by itself or as part of a longer processing sequence, please send us email at
engineering@mems-exchange.org
or call us at (703) 262-5368
SU-8 pre-bake
Material
SU-8
Sides processed
both
Temperature
96 °C
Thermal duration
1 hour
Wafer size
Wafer size
75 mm
100 mm
Equipment
Baking oven
Equipment characteristics:
Wafer geometry
Types of wafers this equipment can accept
no-flat, 1-flat, 2-flat, notched
Wafer holder
Device that holds the wafers during processing.
aluminum plate
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
glass (category), Pyrex (Corning 7740), quartz (single crystal), silicon
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 1500 µm